This analysis shall be made from a test ingot taken during the pouring of the melt. The chemical composition thus determined shall be reported to the purchaser or his representative, and shall conform to the requirements specified in section 2. Railway Age Gazette - Halaman 131917Tampilan utuh - Tentang buku ini
| American Society for Testing Materials - 1920 - 868 halaman
...shall be made by the manufacturer to determine the percentages of the elements specified in Section 3. This analysis shall be made from a test ingot taken...representative, and shall conform to the requirements specified in Section 3. 5. An analysis may be made by the purchaser from a broken tension test specimen... | |
| American Society for Testing Materials - 1912 - 440 halaman
...4. To determine whether the material conforms to the n yses. requirements specified in Section 3, an analysis shall be made from a test ingot taken during the pouring of each melt. A copy of this analysis shall be given to the purchaser or his representative. Check 5.... | |
| 1919 - 382 halaman
...Ladle Analyses, manufacturer to determine the percentages of carbon, manganese, phosphorus and sulfur. This analysis shall be made from a test ingot taken...representative, and shall conform to the requirements specified in Section 3. 5. An analysis may be made by the purchaser from a broken check Analyses, tension... | |
| 1916 - 806 halaman
...made by the manufacturer to determine the percentages of carbon, manganese, phosphorus and sulfur. This analysis shall be made from a test ingot taken during the pouring of the melt. The >NOT>. — The requirements for castings for ships have been especially provided for in the Standard... | |
| George A. Hool, Nathan C. Johnson - 1918 - 1056 halaman
...Phosphorus. Bessemer not over 0 . 10 % Open-hearth not over 0 . 05 % 6. An analysis of each melt of steel shall be made by the manufacturer to determine...representative, and shall conform to the requirements specified in Sort. 5. 7. Analyses may be made by the purchaser from finished bars representing each... | |
| 1918 - 1234 halaman
...over 0.06 per cent. Sulphur Not over 0.045 per cent. Ladle analyses. 3. An analysis of each melt of steel shall be made by the manufacturer to determine...representative, and shall conform to the requirements specified in section 2. Check analyes. 4. Analyses may be made by the purchaser from finished material... | |
| GEORGE A. HOOL,S.B. - 1918 - 982 halaman
...Phosphorus, Bememer not over 0.10% Open-hearth not over 0.05 % 6. An analysis of each melt of steel «hall be made by the manufacturer to determine the percentages...representative, and shall conform to the requirements specified in Sect. 5. 7. Analyses may be made by the purchaser from finished bars representing each... | |
| 1918 - 992 halaman
...Ladle Analyse», manufacturer to determine the percentages of the elements specified in Section 5. This analysis shall be made from a test ingot taken...the melt. The chemical composition thus determined, together with such identifying records as may be desired, shall be reported to the purchaser or his... | |
| George A. Hool, Nathan C. Johnson - 1918 - 924 halaman
...analysis of each melt of steel shall be made by the manufacturer to determine the percentages of carQ. manganese, phosphorus and sulphur. This analysis shall...be made from a test ingot taken during the pouring the melt. The chemical composition thus determined shall be reported to the purchaser or his representative,... | |
| Carnegie Steel Company - 1919 - 456 halaman
...Phosphorusi iBasic " " 0.04 " Sulphur " " 0.045 " " 3. Ladle Analyses. An analysis of each melt of steel shall be made by the manufacturer to determine...representative, and shall conform to the requirements specified in sec. 2. 4. deck Analyses. Analyses may be made by the purchaser from finished bars representing... | |
| |