" If any test specimen shows defective machining or develops flaws, it may be discarded and another specimen substituted. (c) If the percentage of elongation of any tension test specimen is less than that specified in Section 6 (a) and any part of the fracture... "
Railway Age Gazette - Halaman 14
1917
Tampilan utuh - Tentang buku ini

Report of Proceedings of the ... Annual Convention of the ..., Volume 50

American Railway Master Mechanics' Association - 1918 - 678 halaman
...Section 9 (a), and any part of the fracture is more than 34 ln. from the center of the gage length, as indicated by scribe scratches marked on the specimen before testing, a retest shall be allowed. 12. Retests. — (a) If the results of the physical tests of any test lot do not conform to the requirements...
Tampilan utuh - Tentang buku ini

Bulletin, Volume 20,Bagian 1

American Society for Testing Materials - 1920 - 868 halaman
...specified in Section 5 and any part of the fracture is outside the middle third of the gage length, as indicated by scribe scratches marked on the specimen before testing, a retest shall be allowedRetests. 9. If the results of the physical tests of any test lot do not conform to the requirements...
Tampilan utuh - Tentang buku ini

Official Gazette, Volume 97,Masalah 8

Philippines - 2001 - 90 halaman
...than that specified, and any part of the fracture is outside the middle third of the gauge length, as indicated by scribe scratches marked on the specimen before testing, a retest shall be allowed. C3.4 If the results of an original tension test specimen fail to meet the specified minimum requirements...
Tampilan utuh - Tentang buku ini

Transactions of the American Society of Mechanical Engineers, Volume 36

American Society of Mechanical Engineers - 1915 - 1412 halaman
...tension test specimen is less than that specified in Par. 67, and any part of the fracture is more than % in. from the center of the gage length of a 2-in....specimen before testing, a retest shall be allowed. IV PERMISSIBLE VARIATIONS IN GAGE 72 Permissible Variation. The thickness or cross-section of each...
Tampilan utuh - Tentang buku ini

The Design of Steam Boilers and Pressure Vessels

George Bartholomew Haven, George Wright Swett - 1915 - 450 halaman
...specified in Section 6 (a) and any part of the fracture is outside the middle third of the gage length, as indicated by scribe scratches marked on the specimen before testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS IN WEIGHT AND GAGE. 12. When Ordered to Gage. — The thickness of each...
Tampilan utuh - Tentang buku ini

ASME Transactions, Volume 36

American Society of Mechanical Engineers - 1915 - 1466 halaman
...specified in Par. 44 and any part of the fracture is outside the middle third of the gaged length, as indicated by scribe scratches marked on the specimen before testing, a re test shall be allowed. 48 Permissible Variations in Gage. The gage of each bar shall not vary more...
Tampilan utuh - Tentang buku ini

Boiler Safety Orders: Effective January 1, 1917

California. Industrial Accident Commission - 1916 - 170 halaman
...Par. 67, and any part of the fracture is more than % in. from the center of the gage length of a 2-iu. specimen or is outside the middle third of the gage...specimen before testing, a retest shall be allowed. IV PERMISSIBLE VARIATIONS IN GAGE 72 Permissible Variation. The thickness or cross-section of each...
Tampilan utuh - Tentang buku ini

Transactions, Volume 24

American Foundrymen's Society - 1916 - 694 halaman
...Section 9 (a) and any part of the fracture is more than 24-inch from the center of the gage length, as indicated by scribe scratches marked on the specimen before testing, a retest shall be allowed. IV. WORKMANSHIP AND FINISH 14. The castings shall substantially conform to the sizes Wprkmanand shapes...
Tampilan utuh - Tentang buku ini

Concrete Construction for Rural Communities

Roy A. Seaton - 1916 - 246 halaman
...specified in Section 8(a) and any part of the fracture is outside the middle third of the gage length, as indicated by scribe scratches marked on the specimen before testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS IN WEIGHT 13. Permissible Variations. — The weight of any lot of bars...
Tampilan utuh - Tentang buku ini

A.S.T.M. Standards

1916 - 806 halaman
...specified in Section 5 (a) and any part of the fracture is outside the middle third of the gage length, as indicated by scribe scratches marked on the specimen before testing, a re test shall be allowed., — r~| r—1 — *" t A f ** i 1 V • /ttwf2' | "-*^ W i J :* ' 1 w 1...